Wednesday, April 14, 2010

Fwd: MEMS-talk Digest, Vol 90, Issue 9



---------- Forwarded message ----------
From: <mems-talk-request@memsnet.org>
Date: Tue, Apr 13, 2010 at 11:00 AM
Subject: MEMS-talk Digest, Vol 90, Issue 9
To: mems-talk@memsnet.org


Send MEMS-talk mailing list submissions to
       mems-talk@memsnet.org

To subscribe or unsubscribe via the World Wide Web, visit
       http://mail.mems-exchange.org/mailman/listinfo/mems-talk
or, via email, send a message with subject or body 'help' to
       mems-talk-request@memsnet.org

You can reach the person managing the list at
       mems-talk-owner@memsnet.org

When replying, please edit your Subject line so it is more specific
than "Re: Contents of MEMS-talk digest..."

Today's Topics:

  1. wet chemical silicon etch with photoresist mask (10um)
     (Robert MacDonald)


---------- Forwarded message ----------
From: Robert MacDonald <robm@shearwaterscientific.com>
To: mems-talk@memsnet.org
Date: Mon, 12 Apr 2010 00:09:49 -0800
Subject: [mems-talk] wet chemical silicon etch with photoresist mask (10um)
Does anyone know of a reliable wet chemical silicon etch (isotropic or anisotropic) which can be masked by photo resist? I need to etch down 10um.

Rob MacDonald




Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


No comments:

Post a Comment